Patent · US9745205B1 · B1 · US
Non-lithium metal ion battery electrode material architecture
- (11) Publication number
- US9745205B1
- (21) Application number
- 15/626,275
- (22) Filing date
- 2017-06-19
- (30) Priority date
- 2013-05-10
- (43) Publication date
- 2017-08-29
- (45) Date of grant
- 2017-08-29
- (52) CPC
- C01G Compounds containing metals not covered by subclasses C01D or C01F: 39/06, 39/006
- C01P Indexing scheme relating to structural and physical aspects of solid inorganic compounds: 2002/20, 2002/72, 2002/78, 2006/40
- H01M Processes or means, e.g. batteries, for the direct conversion of chemical energy into electrical energy: 4/36, 4/38, 4/581, 4/5815, 4/622
- Y02E Reduction of greenhouse gas [ghg] emissions, related to energy generation, transmission or distribution: 60/10
- (73) Assignee
- UNIV HOUSTON SYSTEM
- (54) Title
- Non-lithium metal ion battery electrode material architecture
- (57) Abstract
A method for configuring a non-lithium-intercalation electrode includes intercalating an insertion species between multiple layers of a stacked or layered electrode material. The method forms an electrode architecture with increased interlayer spacing for non-lithium metal ion migration. A laminate electrode material is constructed such that pillaring agents are intercalated between multiple layers of the stacked electrode material and installed in a battery.
- Full text
- View on Google Patents
Claims (12)
- A method of fabrication and use of a battery electrode, comprising: delaminating an electrode material comprising A x M y N z, exposing the delaminated A x M y N z to a solution containing the insertion species, such that the insertion species intercalate A x M y N z layers; restacking the delaminated A x M y N z around the insertion species to form a battery electrode, wherein restacking comprises forming an electrode of a layered structure comprising A x M y N z, a pillaring agent, and at least one non-lithium metal ion X n+, wherein, in a first state, the layered structure comprises a first layer of A x M y N z a second layer of A x M y N z, and a spacing between the first and the second layers, wherein the pillaring agent and the non-lithium metal ion are disposed between the first layer and the second layer of the A x M y N z; and cycling the battery electrode for a plurality of cycles, wherein, in a second state, subsequent to a plurality of battery electrode cycles, the pillaring agent remains disposed between the first and second layers and the layered structure is configured to maintain the spacing of the first state.
- The method of claim 1, wherein the delaminating A x M y N z electrode material comprises at least one method chosen from the group consisting of physical exfoliation, electrochemical reduction/oxidation, and chemical reduction/oxidation.
- The method of claim 1, wherein the restacking the delaminated A x M y N z around the insertion species comprises at least one method chosen from the group consisting of filtration, centrifugation, drying, or combinations thereof at a temperature ranging from −80° C. to 150° C.
- The method of claim 1, wherein the non-lithium metal ions comprise a formula X n+, wherein X is at least one non-lithium metal chosen from the group consisting of Na, K, Mg, Ca, Al, Ga, and Y, and 1≦n≦3.
- A battery comprising: an electrolyte; and at least one electrode material architecture comprising a layered structure comprising A x M y N z, a pillaring agent, and at least one non-lithium metal ion X n+ wherein the layered structure comprises a first layer of A x M y N z a second layer of A x M y N z, and a spacing between the first and the second layers, wherein the pillaring agent and the non-lithium metal ion are disposed between the first layer and the second layer of the A x M y N z; and wherein the layered structure is configured such that, subsequent to a plurality of battery electrode cycles, the pillaring agent remains disposed between the first and second layers and the spacing between the first and second layers does not change; A is at least one low-valence element chosen from the group consisting of H, alkaline, and alkaline earth metals, and 0≦x≦1.5; M is at least one metal and 1≦y≦2.5; N is at least one non-metal element chosen from the group consisting of O, S, Se, N, P, Br, and I, and 1.8≦z≦4.2; and X is at least one non-lithium metal ion chosen from the group consisting of Na, K, Mg, Ca, Al, Ga, and Y, and 1≦n≦3.
- The battery of claim 5, wherein a low-valence element further comprises at least one chosen from the group consisting of Li, Na, K, Mg, and Ca.
- The battery of claim 5, wherein at least one metal comprises a metal chosen from the group consisting of Ti, Zr, V, Ta, Cr, Mo, W, Mn, Fe, Co, Ni, Cu, Zn, Cd, Ga, In, Sn, Pb, Sb, Bi, and Te.
- The battery of claim 5, wherein the pillaring agent comprises at least one electrically neutral polymer containing O, N, F, and/or S atoms chosen from the group consisting of poly(ethylene oxide), poly(propylene glycol), poly(vinylpyrrolidinone), methyl cellulose, poly(methyl acrylate), polyacrylonitrile, polyethyleneimine, poly(aniline), and polypyrrole.
- The battery of claim 5, wherein the pillaring agent comprises at least one electrically neutral molecule containing O, N, F, and/or S atoms chosen from the group consisting of alkylamines and glymes.
- The battery of claim 9, wherein the alkylamines comprise at least one molecule chosen from the group consisting of diethylamine, dibutylamine, dipentylamine, N-isopropylcyclohexylamine, and dicyclohexylamine.
- The battery of claim 9, wherein the glymes consist of at least one molecule chosen from the group consisting of diglyme, triglyme, and tetraglyme.
- The battery of claim 5, wherein the non-lithium metal ions are positioned within the lattice spacing of A x M y N z and induce a lattice expansion of 1-300% in at least one dimension.