MLchartDataset catalogue

Patent · US10040993B1 · B1 · US

Chemiluminescent materials and method of making same

(11) Publication number
US10040993B1
(21) Application number
15/586,704
(22) Filing date
2017-05-04
(30) Priority date
2016-05-19
(43) Publication date
2018-08-07
(45) Date of grant
2018-08-07
(52) CPC
  • C09K Materials for miscellaneous applications, not provided for elsewhere: 11/07
  • B01J Chemical or physical processes, e.g. catalysis or colloid chemistry; their relevant apparatus: 13/04, 13/14, 13/185
  • C09B Organic dyes or closely-related compounds for producing dyes {, e.g. pigments}; mordants; lakes: 3/36, 67/0097
  • F21K Non-electric light sources using luminescence; light sources using electrochemiluminescence; light sources using charges of combustible material; light sources using semiconductor devices as light-generating elements; light sources not otherwise provided for: 2/06
(73) Assignee
US AIR FORCE
(54) Title
Chemiluminescent materials and method of making same
(57) Abstract

Chemiluminescent materials are provided that include an encapsulated oxalate-containing composition that includes a core portion and a polymeric coating, a peroxide source, and a fluorescent dye. The core portion includes an oxalate; a polymerizable component composition that polymerizes upon exposure to ultraviolet radiation; a photosensitizer; and an ultraviolet screening agent. The polymeric coating layer surrounding the core portion comprises a polymer derived from the polymerizable component composition. A fluorescent dye may be intermixed in the oxalate-containing composition, intermixed with the peroxide source, present in the chemiluminescent material as a separate dye layer or particle, or present within another component of the chemiluminescent material. A method for making the chemiluminescent material is also provided.

Full text
View on Google Patents

Claims (19)

  1. A chemiluminescent material comprising an encapsulated oxalate-containing composition, comprising: a core portion comprising the oxalate-containing composition comprising: an oxalate; a polymerizable component composition comprising one or more monomers and/or oligomers that polymerize upon exposure to ultraviolet radiation, wherein the one or more monomers and/or oligomers is selected from the group consisting of acrylate monomers, acrylate oligomers, methacrylate monomers, methacrylate oligomers, and combinations thereof; a photosensitizer; and an ultraviolet (UV) screening agent; a polymeric coating layer surrounding the core portion, wherein the polymeric coating layer comprises a polymer derived from the polymerizable component composition; a peroxide source; and a fluorescent dye.
  2. The chemiluminescent material of claim 1, wherein the oxalate is an oxalic-type diester having a typical formula: R 1 - O 2 C - CO 2 - R 2 wherein, R 1 and R 2 are independently selected from the group consisting of an unsubstituted aryl group, a substituted aryl group, and an unsaturated alkane group.
  3. The chemiluminescent material of claim 2, wherein the substituted aryl groups is selected from the group consisting of chlorophenyl, dichlorophenyl, trichlorophenyl, nitrophenyl, dinitrophenyl, benzoylxyphenyl, formylphenyl, carboxyphenyl, methoxyphenyl, acetylaminophenyl, pyridylphenyl, sulfophenyl, 2,4,5-trichloro-6-carbopentoxyphenyl, and 2-carbopentyloxy-3,5,6-trichlorophenyl; and wherein the unsaturated alkane group is selected from the group consisting of vinyl, 2-propenyl, 2-octenyl, (1-phenyl)vinyl, 1-cyclohexenyl, and 1-cyclooctenyl.
  4. The chemiluminescent material of claim 1, wherein the oxalate is selected from the group consisting of diphenyl oxalate; bis(2,4,6-trichlorophenyl)oxalate; bis(2,4,5-trichloro-6-(pentyloxycarbonyl)phenyl)oxalate; bis(2-carbopentyloxy-3,5,6-trichlorophenyl)oxalate; bis(2,4,5-tribromo-6-carbohexyloxyphenyl)oxalate; bis(2-nitrophenyl)oxalate; bis(2,4-dinitrophenyl)oxalate; bis(2,6-dichloro-4-nitrophenyl) oxalate; bis(3-trifluoromethyl-4-nitrophenyl)oxalate; bis(2-methyl-4,6-dinitrophenyl)oxalate; bis(1,2-dimethyl-4,6-dinitrophenyl)oxalate; bis(2,4-dichlorophenyl)oxalate; bis(2,4-dinitrophenyl)oxalate; bis(2,5-dinitrophenyl)oxalate; bis(2-formyl-4-nitrophenyl)oxalate; bis(pentachlorophenyl)oxalate; bis(1,2-dihydro-2-oxo-1-pyridyl)glyoxal; bis(2,4-dinitro-6-methylphenyl)oxalate; bis-N-phthalimidyl oxalate; bis(vanillyl)oxalate; bisvinyl oxalate; bisallyl oxalate; bis(2-propenyl)oxalate; bis(2-octenyl)oxalate; bis(1-phenyl)vinyl oxalate; 1-cyclohexenyl oxalate; and 1-cyclooctenyl oxalate.
  5. The chemiluminescent material of claim 1, wherein the polymerizable component composition comprises a mono-functional monomer, a di-functional monomer, or multi-functional compound, wherein a polymerizable functional group is an alpha, beta-unsaturated carbonyl compound.
  6. The chemiluminescent material of claim 1, wherein the polymerizable component composition comprises: about 2 wt % to about 40 wt % of a mono-functional monomer; about 2 wt % to about 40 wt % of a di-functional monomer; and about 4 wt % to about 50 wt % of a multi-functional compound, wherein wt % is based on a total weight of the polymerizable component mixture.
  7. The chemiluminescent material of claim 1, wherein the fluorescent dye is intermixed in the oxalate-containing composition, intermixed with the peroxide source, present as a separate dye layer or particle, or present within another component of the chemiluminescent material.
  8. The chemiluminescent material of claim 1, wherein the UV screening agent is a UV light absorber selected from the group consisting of p-t-butylphenyl salicylate; benzophenone; 2,4-dihydroxybenzophenone; 2-hydroxy-4-methoxybenzophenone; 2-hydroxy-4-octoxybenzophenone; 2(2′-hydroxy-4′-octoxyphenyl)benzotriazole, and a vat dye.
  9. The chemiluminescent material of claim 8, wherein UV screening agent is the vat dye, wherein the vat dye is violanthrone or a violanthrone derivative.
  10. The chemiluminescent material of claim 9, wherein the UV screening agent comprises the chemiluminescent dye as a substructure, and wherein the vat dye is an alkyloxy-violanthrone derivative.
  11. The chemiluminescent material of claim 1, wherein the peroxide source forms an exterior peroxide coating on an exterior surface of the polymeric coating layer.
  12. A method of preparing a chemiluminescent material comprising an encapsulated oxalate-containing composition, the method comprising the steps of: dispersing an oxalate-containing composition in a fluid medium to form particles as a dispersed phase in a continuous phase of the fluid medium, the oxalate-containing composition comprising: an oxalate; a polymerizable component composition comprising one or more monomers and/or oligomers that polymerize upon exposure to ultraviolet radiation, wherein the one or more monomers and/or oligomers is selected from the group consisting of acrylate monomers, acrylate oligomers, methacrylate monomers, methacrylate oligomers, and combinations thereof; a photosensitizer; and an ultraviolet screening agent; and exposing the particles to ultraviolet radiation to induce polymerization of the polymerizable component composition at a surface region of the particles thereby forming polymeric coatings around the particles to form the encapsulated oxalate-containing composition, wherein a capsule of the encapsulated oxalate-containing composition comprises a core region that includes an uncured portion of the oxalate-containing composition encapsulated by a polymeric coating layer; and combining the encapsulated oxalate-containing composition with a peroxide source, wherein a fluorescent dye is intermixed in the oxalate-containing composition, intermixed with the peroxide source, present as a separate dye layer or particle, or present within another component of the chemiluminescent material.
  13. The method according to claim 12, wherein the photosensitizer is present in an amount of about 0.1 to about 20 parts per 100 parts by weight of the polymerizable composition.
  14. The method according to claim 12, wherein the ultraviolet screening agent is selected from the group consisting of oil-screening soluble dyes, loading and color pigments, and ultraviolet light absorbers.
  15. The method according to claim 12, wherein the ultraviolet screening agent is present in an amount of about 0.1 to about 20 parts per 100 parts by weight of the polymerizable composition.
  16. The method according to claim 12, wherein the fluid medium comprises an aqueous solution; and wherein the plurality of monomers or oligomers comprises hydrophobic compounds.
  17. The method according to claim 16, wherein the aqueous solution comprises water and a water-soluble dispersing agent present in an amount of about 1 wt % to about 10 wt %, wherein wt % is based on a total mass of the aqueous solution.
  18. The method according to claim 12, wherein exposing the particles to ultraviolet radiation is performed for a period of about 1 minute to about 30 minutes at a power of between about 500-1500 mJ/cm 2.
  19. The method according to claim 12, wherein the fluid medium comprises a gaseous medium.