MLchartDataset catalogue

Patent · US4973372A · A · US

Method of making a tie-bar with internal lubrication

(11) Publication number
US4973372A
(21) Application number
07/383,672
(22) Filing date
1989-07-24
(30) Priority date
1984-08-29
(43) Publication date
1990-11-27
(45) Date of grant
1990-11-27
(51) IPC
B29C 53/56; F16C 7/00
(52) CPC
  • B29C Shaping or joining of plastics; shaping of material in a plastic state, not otherwise provided for; after-treatment of the shaped products, e.g. repairing: 53/56
  • B29L Indexing scheme associated with subclass B29C, relating to particular articles: 2031/75
  • B60G Vehicle suspension arrangements: 2206/11, 2206/7101
  • F16C Shafts; flexible shafts; elements or crankshaft mechanisms; rotary bodies other than gearing elements; bearings: 7/026
  • Y10S Technical subjects covered by former uspc cross-reference art collections [xracs] and digests: 464/903
  • Y10T Technical subjects covered by former us classification: 74/2142
(73) Assignee
AlliedSignal Inc
(72) Inventors
Richard J. Ditlinger
(54) Title
Method of making a tie-bar with internal lubrication
(57) Abstract

The tie-bar (10) comprises a pair of spaced-apart bushings (12, 14) each having end flanges (16) extending from a central cylindrical portion and a through opening (18) for connecting to flexing structures. A plurality of wires (20) comprises bands (22) of parallel wires (20) wrapped endlessly about the spaced-apart bushings (12, 14) provide a tie-bar (10) having bushings (12, 14) disposed at the ends and connected by a pair of spaced-apart side portions (24) of superimposed bands (22). The wires (20) are coated with a dry film lubricant so that the wires (20) are dry wrapped about the bushings (12, 14), and then a resin material (23) encapsulated about the dry wrapped wire bands (22) and bushings (12, 14). A body (26) of resin material disposed between the spaced-apart side portions (24) and the bushings (12, 14) maintains the spaced-apart relationship of the bushings (12, 14) by withstanding the compressive tension of the tightly wrapped wires (20). The wires (20) are free to move relative to one another in response to tension and torsional forces exerted upon the tie-bar (10).

Full text
View on Google Patents

Claims (6)

  1. A method for making a tension-torsion tie-bar of dry film lubricant-coated filaments, a non-carcinogenic adhesive material disposed about and between bushings and parallel spaced-apart side portions of band formation of the filaments, the bushings and spaced-apart side formations defining an area therebetween and adhesive material filling completely the area to provide a body of material for maintaining compressive tension between said bushings by keeping the bushings in spaced-apart relationship to one another, the filaments disposed closely adjacent to one another and to filaments of adjacent superimposed band formations, the adhesive material extending to and surrounding perimeters of the side portions and not extending between adjacent filaments and superimposed band formations so that tension-torsion forces exerted on the tie-bar effect movement of the filaments relative to one another without restraint thereof by said adhesive material, comprising the steps of: drawing said dry film lubricant-coated filaments form uniformly rotating spools; drawing said filaments through a die to arrange each of said filaments parallel to each other in a band formation; attaching an end of the band formation to one of two spaced-apart flanged bushings in a rotating fixture; rotating said fixture to wrap the band formations about each of the bushings and between the flanges thereof; cutting the band formation of filaments when a sufficient number of layers thereof have been wrapped about said bushings to form a lamination of band formations; securing the loose end of said band formation of filaments; performing one of the steps selected from the group consisting of (a) keeping said fixture, bushings, and lamination until said lamination is to be encapsulated in said non-carcinogenic adhesive material, and (b) encapsulating the lamination of band formations by application of the adhesive material thereabout and curing to polymerize the material.
  2. The method of accordance with claim 1, wherein noncoated filaments are drawn from said spools and then coated with a dry film lubricant comprising one of graphite and molybdenum disulfite.
  3. The method in accordance with claim 1, wherein said adhesive material comprises a low modulus urethane.
  4. The method is accordance with claim 1, wherein said adhesive material filling said area provides a singular mechanism which keeps the bushings in spaced-apart relationship and maintains structural stability of the tie-bar.
  5. The method in accordance with claim 1, wherein said adhesive material is chosen from a group consisting of a reaction injected molded elastomeric urethene, an elastomeric thermoplastic, and a thermosetting urethane.
  6. The method in accordance with claim 1, wherein said dry film lubricant is chosen from a group consisting of graphite and molybdenum disulfite.

Description

This is a divisional of co-pending application Ser. No. 06/804,231 filed on Dec. 3, 1985, now U.S. Pat. No. 4873889 which is a continuation of abandoned application Ser. No. 06/645,210 filed Aug. 24, 1984.

The present invention relates to a tie-bar with internal lubrication between individual wire strands of the assembly whereby the wire strands are free to move relative to one another as a result of axial and torsional forces exerted thereon.

It has been the practice to make structures subjected to high tensile and torsional loading, for example the connecting members or tie-bars between helicopter rotor blades and the driving rotor, from a pair of metal bushings connected together by endless strands of parallel wires secured together by an adhesive resin such as urethane, with the resin disposed between each of the wires. Such urethane impregnated tie-bar assemblies are illustrated in U. S. Pat. Nos. 3,434,899 and 3,460,628 issued to James A. Tankersley on Mar 25, 1969 and Aug. 12, 1969, respectively, and both assigned to the same assignee as herein. Urethane impregnated tie-bar assemblies present a number of problems in their manufacture and use. The tie-bar is wet wrapped during the assembly process and the urethane material comprises a carcinogenic material which requires that workers wear protective clothing in an enclosed area because of the inherent dangers.