MLchartDataset catalogue

Patent · US5701948A · A · US

Casting steel strip

(11) Publication number
US5701948A
(21) Application number
08/633,949
(22) Filing date
1996-04-17
(30) Priority date
1995-05-05
(43) Publication date
1997-12-30
(45) Date of grant
1997-12-30
(51) IPC
B22D 11/00; B22D 11/04; B22D 11/059; B22D 11/06
(52) CPC
  • B22D Casting of metals; casting of other substances by the same processes or devices: 11/0651, 11/00
(73) Assignee
BHP Steel JLA Pty Ltd; IHI Corp
(72) Inventors
Lazar Strezov; Rama Ballav Mahapatra; Fred de Sylva; Kannappar Mukunthan
(54) Title
Casting steel strip
(57) Abstract

In continuous casting of steel strip, a casting pool of molten metal is supported on moving casting surfaces which are chilled to cause solidification of steel on the casting surfaces. The casting surfaces are textured by provision of parallel groove and ridge formations (11) defining V-shaped grooves (12) and ridges (13) with sharp edges (14). The depth (d) of the texture from ridge peak to groove root is in the range 5 to 50 microns and the pitch (p) between the grooves is in the range 100 to 250 microns. The casting surfaces may be peripheral surfaces of casting rolls of a twin roll caster.

Full text
View on Google Patents

Claims (24)

  1. A method of continuously casting steel strip comprising supporting a casting pool of molten steel on one or more chilled casting surfaces and moving the chilled casting surface or surfaces to produce a solidified strip moving away from the casting pool, wherein the or each casting surface is textured by the provision of parallel groove and ridge formations of essentially constant depth and pitch, the depth of the texture from ridge peak to groove root being in the range 5 microns to less than 50 microns, and said pitch being in the range 100 to 250 microns.
  2. A method as claimed in claim 1, wherein the casting pool is supported on peripheral casting surfaces of a pair of chilled casting rolls forming a nip between them and rotated in mutually opposite directions to produce the solidified strip such that it moves downwardly from the nip.
  3. A method as claimed in claim 2, wherein the groove and ridge formations in each casting surface are defined by a series of parallel annular grooves extending circumferentially around the casting surface and regularly spaced longitudinally of the casting surface at said pitch.
  4. A method as claimed in claim 3, wherein the groove and ridge formations in each casting surface are defined by one or more grooves extending helically of the casting surface.
  5. A method as claimed in claim 1, wherein the groove formations are of substantially V-shaped cross-section and the ridge formations have sharp circumferential edges.
  6. A method as claimed in claim 1, in which the depth of the texture is in the range 15 to 25 microns and said pitch is between 150 and 200 microns.
  7. A method as claimed in claim 6, wherein the depth of the texture is about 20 microns and said pitch is about 180 microns.
  8. A method as claimed in claim 1, wherein the casting surfaces are chromium surfaces.
  9. A method as claimed in claim 1, wherein the molten steel has a sulphur content of at least 0.02%.
  10. A method as claimed in claim 9, wherein the molten steel is a silicon/manganese killed steel having a manganese content of not less than 0.20% and a silicon content of not less than 0.10% by weight.
  11. A method as claimed in claim 9, wherein the sulphur content of the steel is no less than 0.03% by weight.
  12. A method as claimed in claim 11, wherein the sulphur content of the steel is in the range 0.03 to 0.07% by weight.
  13. A method as claimed in claim 1, wherein the casting pool is supported on peripheral casting surfaces of a pair of chilled casting rolls forming a nip between them and rotated in mutually opposite directions to produce the solidified strip such that it moves downwardly from the nip. The groove and ridge formations extend circumferentially of the casting surfaces of the rolls, the groove formations are of substantially V-shaped cross-sections and the ridge formations have sharp circumferential edges.
  14. A method as claimed in claim 13, wherein the depth of the texture is in the range 15 to 25 microns and said pitch is between 150 and 200 microns.
  15. A method as claimed in claim 14, wherein the depth of the texture is about 20 microns and said pitch is about 180 microns.
  16. A method as claimed in claim 13, wherein the casting surfaces are chromium surfaces.
  17. A method as claimed in claim 13, wherein the molten steel has a sulphur content of at least 0.02%.
  18. A method as claimed in claim 16, wherein the molten steel is a silicon/manganese killed steel having a manganese content of not less than 0.02% and a silicon content of not less than 0.10% by weight.
  19. Apparatus for continuously casting steel strip comprising a pair of casting rolls forming a nip between them, a metal delivery nozzle for delivery of molten steel into the nip between the casting rolls to form a casting pool of molten metal supported on casting roll surfaces immediately above the nip, and roll drive means to drive the casting rolls in counter-rotational directions to produce a solidified steel strip delivered downwardly from the nip, wherein the casting surfaces of the rolls are textured by the provision of circumferentially extending groove and ridge formations of constant depth and pitch, the depth of the texture from ridge peak to groove root being in the range 5 microns to less than 50 microns, and said pitch being in the range 100 to 250 microns.
  20. Apparatus as claimed in claim 19, wherein the groove and ridge formations in each casting surface are defined by a series of parallel annular grooves extending circumferentially around the casting surface and regularly spaced longitudinally of the casting surface at said pitch.
  21. Apparatus as claimed in claim 19, wherein the groove and ridge formations in each casting surface are defined by one or more grooves extending helically of the casting surface.
  22. Apparatus as claimed in claim 19, wherein the grooves of the casting surfaces are of substantially V-shaped cross-section and the ridge formations have sharp circumferential edges.
  23. Apparatus as claimed in claim 19, wherein the depth of the texture of the casting surfaces is in the range 15 to 25 microns and said pitch is between 150 and 200 microns.
  24. Apparatus as claimed in claim 23, wherein the depth of the texture in the casting surfaces is about 20 microns and said pitch is about 180 microns.

Description

This invention relates to the casting of steel strip.

It is known to cast metal strip by continuous casting in a twin roll caster. In this technique molten metal is introduced between a pair of contra-rotated horizontal casting rolls which are cooled so that metal shells solidify on the moving roll surfaces end are brought together at the nip between them to produce a solidified strip product delivered downwardly from the nip between the rolls. The term "nip" is used herein to refer to the general region at which the rolls are closest together. The molten metal may be poured from a ladle into a smaller vessel from which it flows through a metal delivery nozzle located above the nip so as to direct it into the nip between the rolls, so forming a casting pool of molten metal supported on the casting surfaces of the rolls immediately above the nip and extending along the length of the nip. This casting pool is usually confined between side plates or dams held in sliding engagement with end surfaces of the rolls so as to dam the two ends of the casting pool against outflow, although alternative means such as electromagnetic barriers have also been proposed.

Although twin roll casting has been applied with some success to non-ferrous metals which solidify rapidly on cooling, there have been problems in applying the technique to the casting of ferrous metals. One particular problem has been the achievement of sufficiently rapid and even cooling of metal over the casting surfaces of the rolls.