MLchartDataset catalogue

Patent · US9873165B2 · B2 · US

Piston rod manufacturing method

(11) Publication number
US9873165B2
(21) Application number
14/914,006
(22) Filing date
2014-08-11
(30) Priority date
2013-08-26
(43) Publication date
2018-01-23
(45) Date of grant
2018-01-23
(51) IPC
B23K 20/12; B23K 31/12; B23P 15/10; F16J 7/00; F15B 15/14; F16C 7/02
(52) CPC
  • B23K Soldering or unsoldering; welding; cladding or plating by soldering or welding; cutting by applying heat locally, e.g. flame cutting; working by laser beam: 20/12, 20/129, 2101/003, 2201/003, 31/125
  • B23P Metal-working not otherwise provided for; combined operations; universal machine tools: 15/10
  • F15B Systems acting by means of fluids in general; fluid-pressure actuators, e.g. servomotors; details of fluid-pressure systems, not otherwise provided for: 15/1457
  • F16C Shafts; flexible shafts; elements or crankshaft mechanisms; rotary bodies other than gearing elements; bearings: 2226/36, 7/023
  • F16J Pistons {}; cylinders; sealings: 7/00
(73) Assignee
KYB YS Co Ltd
(72) Inventors
Nobuyuki Kobayashi
(54) Title
Piston rod manufacturing method
(57) Abstract

A piston rod manufacturing method of manufacturing a piston rod by joining a solid rod main body and a solid rod head includes a first step of joining respective end surfaces of the rod main body and the rod head by friction welding; and a second step of performing boring process on an axial center portion from the rod head side so as to penetrate through a joining face between the rod main body and the rod head.

Full text
View on Google Patents

Claims (3)

  1. A piston rod manufacturing method of manufacturing a piston rod by joining a solid rod main body and a rod head having an annular clevis connected to a load and a solid body portion, comprising: a first step of joining an end surface of the rod main body and an end surface of the body portion of the rod head at a joining face by friction welding; and a second step of performing a boring process on an axial center portion from the rod head side so as to form a hole that penetrates from the rod head side through the clevis and the joining face and into the rod main body; wherein the second step is performed after the first step.
  2. The piston rod manufacturing method according to claim 1, further comprising a third step of sealing at least one of respective holes formed in the clevis and in the body portion in the second step with a sealing member.
  3. The piston rod manufacturing method according to claim 1, further comprising a step of performing a quality inspection by means of a nondestructive test on a friction-welded portion between the rod main body and the rod head after the first step and before the second step.

Description

The present invention relates to a piston rod manufacturing method.

A rod main body and a rod head are generally manufactured by processing a steel material manufactured by continuous casting. Impurities caused by center segregation exist in a central portion of the steel material manufactured by the continuous casting. Therefore, there is a risk that delayed fracture is caused at a center segregation portion if the rod main body and the rod head are joined by friction welding.

JP2011-56531A discloses a piston rod manufacturing method including a step of hollowing out respective axial center portions of a rod main body and a rod head from respective end surfaces thereof to remove impurities caused by center segregation, and a step of joining the respective end surfaces of the rod main body and the rod head by friction welding.

Accordance to the piston rod manufacturing method disclosed in JP2011-56531A, the respective end surfaces of the rod main body and the rod head are joined integrally by friction welding after the impurities existing in the axial center portion have been removed, and thereby, it is possible to manufacture a piston rod having the joining face with no impurities. Therefore, in accordance with the piston rod manufacturing method disclosed in JP2011-56531A, it is possible to improve the joint strength between the rod main body and the rod head.