Patent · US5563734A · A · US
Durable low-emissivity solar control thin film coating
- (11) Publication number
- US5563734A
- (21) Application number
- 08/337,686
- (22) Filing date
- 1994-11-10
- (30) Priority date
- 1993-04-28
- (43) Publication date
- 1996-10-08
- (45) Date of grant
- 1996-10-08
- (51) IPC
- C03C 17/36; G02B 5/28
- (52) CPC
- C03C Chemical composition of glasses, glazes or vitreous enamels; surface treatment of glass; surface treatment of fibres or filaments made from glass, minerals or slags; joining glass to glass or other materials: 17/3618, 17/36, 17/3626, 17/3644, 17/366, 17/3681, 2217/24, 2217/242, 2217/78
- G02B Optical elements, systems or apparatus: 5/282
- (73) Assignee
- BOC Group Inc
- (72) Inventors
- Jesse D. Wolfe; Abraham I. Belkind; Ronald E. Laird
- (54) Title
- Durable low-emissivity solar control thin film coating
- (57) Abstract
An infrared reflecting interference filter capable of transmitting a desired proportion of visible radiation while reflecting a large portion of incident solar radiation is provided. The filter comprises a transparent substrate onto which is deposited a dielectric layer, followed by metal and dielectric layers. In between each of the dielectric and metal layers is deposited a precoat layer that promotes adhesion between the dielectric and the metal. One aspect of the invention is the use of a film comprising nickel and chromium nitride for each of the metal precoat layers. These precoat layers are thin so that there is less absorption of visible light but yet maintains good adhesive properties. Another aspect of the invention is the use of silver as the metal layer. Specifically, silver is sputtered in an atmosphere containing a mixture of nitrogen and argon or other inert gas. It was found that the presence of nitrogen produces a silver layer that is more durable than silver films sputtered in an atmosphere containing essentially pure inert gas. In one embodiment, the interference filter comprises a glass substrate onto which is deposited a thin-film design consisting of five layers, namely: titanium dioxide, nickel-chromium nitride, silver, nickel-chromium nitride, and silicon nitride.
- Full text
- View on Google Patents
Claims (29)
- A thin film interference filter comprising: a transparent substrate; a first substantially transparent dielectric layer comprising titanium dioxide; a first metal precoat layer wherein said first metal precoat layer comprises a material selected from the group consisting of the combination of nickel with chromium and the combination of nickel with chromium nitride; a partially reflective metal layer; a second metal precoat layer comprising a mixture of nickel metal and chromium nitride; and a second substantially transparent dielectric layer.
- The thin film interference filter as defined in claim 1 wherein the second dielectric layer comprises silicon nitride.
- The thin film interference filter as defined in claim 2 wherein the partially reflective metal layer comprises silver.
- The thin film interference filter as defined in claim 3 wherein the first dielectric layer has a refractive index of approximately 1.5 to 2.5.
- The thin film interference filter as defined in claim 1 wherein the first metal precoat layer has a thickness of approximately 5 to 20 Å and the second metal precoat layer has a thickness of approximately 5 to 20 Å.
- The thin film interference filter as defined in claim 5 wherein the partially reflective metal layer comprises silver and has a thickness of approximately 80 to 150 Å.
- The thin film interference filter as defined in claim 6 wherein the first dielectric layer has a thickness of approximately 250 to 450 Å and the second dielectric layer has a thickness of approximately 300 to 500 Å.
- The thin film interference filter as defined in claim 7 wherein the first metal precoat layer comprises nickel metal and chromium nitride and has a thickness of approximately 5 to 20 Å, wherein the second metal precoat layer has a thickness of approximately 5 to 20 Å, and wherein the silver metal layer has a thickness of 90 to 150 Å.
- The thin film interference filter as defined in claim 1 wherein the second dielectric layer comprises a composite of silicon nitride and one or more other nitrides selected from the group consisting of zirconium nitride, titanium nitride, and hafnium nitride.
- The thin film interference filter as defined in claim 9 wherein the partially reflective metal layer is a metal selected from the group consisting of silver, gold, copper, and platinum.
- The thin film interference filter as defined in claim 10 wherein the first dielectric layer has a refractive index within a range of approximately 1.5 to 2.5.
- The thin film interference filter as defined in claim 10 wherein the first metal precoat layer has a thickness of approximately 5 to 20 Å and the second metal precoat layer has a thickness of approximately 5 to 20 Å.
- The thin film interference filter as defined in claim 12 wherein the metal layer has a thickness of approximately 90 to 150 Å.
- The thin film interference filter as defined in claim 13 wherein the first dielectric layer has a thickness of approximately 250 to 450 Å and the second dielectric layer has a thickness of approximately 300 to 500 Å.
- The thin film interference filter as defined in claim 14 wherein the second dielectric layer comprises approximately 50 to 100 percent by weight silicon nitride.
- The thin film interference filter as defined in claim 15 wherein the first metal precoat layer comprises nickel and chromium nitride and has a thickness of approximately 5 to 20 Å, wherein the second metal precoat layer has a thickness of approximately 5 to 20 Å, and wherein the partially reflective metal layer comprises silver having a thickness of 90 to 150 Å.
- A method for the production of a durable thin film interference filter on a transparent substrate comprising the steps, in sequence, of: depositing a first substantially transparent dielectric layer comprising titanium dioxide onto said substrate; depositing a first metal precoat layer wherein said first metal precoat layer comprises a material selected from the group consisting of the combination of nickel with chromium and the combination of nickel with chromium nitride; depositing a partially reflective metal layer; depositing a second metal precoat layer comprising a mixture of nickel metal and chromium nitride; and depositing a second substantially transparent dielectric layer.
- The method for the production of a durable thin film interference filter as defined in claim 17 wherein the step of depositing the second metal precoat layer comprises the step of providing a magnetron having a nickel-chromium alloy target and reactively sputtering in an atmosphere containing nitrogen.
- The method for the production of a durable thin film interference filter as defined in claim 18 wherein the first metal precoat layer comprises nickel and chromium nitride and wherein the step of depositing the first metal precoat layer comprises the step of providing a magnetron having a nickel-chromium alloy target and reactively sputtering in an atmosphere containing nitrogen.
- The method for the production of a durable thin film interference filter as defined in claim 19 wherein the partially reflective metal layer comprises silver that is sputtered in an atmosphere containing nitrogen from a silver target of a magnetron.
- The method for the production of a durable thin film interference filter as defined in claim 20 wherein the second dielectric layer comprises silicon nitride.
- The method for the production of a durable thin film interference filter as defined in claim 21 wherein the first metal precoat layer has a thickness of approximately 5 to 20 Å and the second metal precoat layer has a thickness of approximately 5 to 20 Å.
- The method for the production of a durable thin film interference filter as defined in claim 22 wherein the metal layer has a thickness of approximately 90 to 150 Å.
- The method for the production of a durable thin film interference filter as defined in claim 23 wherein the silicon nitride second dielectric layer is deposited by: (a) providing a cylindrical magnetron having a rotatable target comprising silicon and having magnetic means disposed at an angle of approximately 20° to 60° from normal relative to said substrate; and (b) moving said substrate towards the rotatable target so that dielectric material reactively sputtered in an atmosphere containing nitrogen is focused onto the substrate at an acute angle as the substrate approaches the target.
- A method for the production of a durable thin film interference filter on a transparent substrate comprising the steps, in sequence, of: depositing a first substantially transparent dielectric layer onto said substrate; depositing a first metal precoat layer wherein said first metal precoat layer comprises a material selected from the group consisting of the combination of nickel with chromium and the combination of nickel with chromium nitride; depositing a partially reflective metal layer; depositing a second metal precoat layer comprising a mixture of nickel metal and chromium nitride; and depositing a second substantially transparent dielectric layer comprising the steps of: (a) providing a cylindrical magnetron having a rotatable target and having magnetic means disposed at an angle of approximately 20° to 60° from normal relative to said substrate; and (b) moving said substrate towards the rotatable target so that dielectric material is reactively sputtered and focused onto the substrate at an acute angle as the substrate approaches the target.
- The method for the production of a durable thin film interference filter as defined in claim 25 wherein the first dielectric layer comprises titanium dioxide or niobium oxide.
- The method for the production of a durable thin film interference filter as defined in claim 25 wherein the first dielectric layer comprises a nitride selected from the group consisting of silicon nitride, titanium nitride, hafnium nitride, and zirconium nitride and wherein the first dielectric layer is deposited by: (a) providing a cylindrical magnetron having a rotatable target comprising silicon and one or more metals selected from the group consisting of zirconium, titanium, and hafnium and having magnetic means disposed at an angle of approximately 20° to 60° from normal relative to said substrate; and (b) moving said substrate towards the rotatable target so that dielectric material reactively sputtered in an atmosphere containing nitrogen is focused onto the substrate at an acute angle as the substrate approaches the target.
- The method for the production of a durable thin film interference filter as defined in claim 27 wherein the second dielectric layer comprises silicon nitride.
- The method for the production of a durable thin film interference filter as defined in claim 25 wherein the second dielectric layer comprises silicon nitride.
Description
This is a continuation of application Ser. No. 08/054,521, filed Apr. 28, 1993 now abandoned.
This invention relates generally to visibly transparent infrared reflecting interference filters, and more particularly, to a durable low-emissivity filter.
The use of transparent panels in buildings, vehicles and other structures for controlling solar radiation is quite prevalent today. The goal of solar control is to transmit light while excluding much of the solar energy, thus decreasing the amount of air condition or cooling required, and conserving energy. In addition, modified glass as a structural material provides the color flexibility architects desire.
Various processes have been employed to alter the optical properties of these panels, including coating glass or plastic substrates by various techniques such as electrolysis, chemical vapor deposition and physical vapor deposition, including sputtering with planar magnetrons. For instance, thin metal films have been deposited on glass or plastic to increase the reflectance of solar radiation. Windows deposited with a multi-layer dielectric-metal-dielectric coating that exhibits high visible transmittance, and high reflectivity and low emissivity in the infrared range, are even more energy efficient. The index of refraction of the dielectric layer is preferably 2.0 or greater in order to minimize the visible reflectance and enhance the visible transmittance of the window. This dielectric layer which often consists of metal oxide coating also offers additional protection to the fragile metal films.