Patent · US6140405A · A · US
Salt-modified electrostatic dissipative polymers
- (11) Publication number
- US6140405A
- (21) Application number
- 09/157,460
- (22) Filing date
- 1998-09-21
- (30) Priority date
- 1998-09-21
- (43) Publication date
- 2000-10-31
- (45) Date of grant
- 2000-10-31
- (51) IPC
- C08K 3/00; C08K 5/00; C08L 101/00; C08L 67/00; C08L 75/08; C08L 77/12; H10W 42/60
- (52) CPC
- H10W Generic packages, interconnections, connectors or other constructional details of devices covered by class H10: 42/60, 74/47
- C08J Working-up; general processes of compounding; after-treatment not covered by subclasses C08B, C08C, C08F, C08G or C08H: 7/12
- C08K Use of inorganic or non-macromolecular organic substances as compounding ingredients: 3/01
- (73) Assignee
- BF Goodrich Corp
- (72) Inventors
- Yona Eckstein; Ramakrishna Ravikiran
- (54) Title
- Salt-modified electrostatic dissipative polymers
- (57) Abstract
A low molecular weight polyether oligomer is modified with a salt during chain extending reaction of the polyether oligomer to form electrostatic dissipative polymer products such as polyurethanes, polyether amide block copolymers and polyether-ester block copolymers. The reaction product polymers exhibit relatively low surface and volume resistivities, and static decay times which are not too fast or too slow, yet are free of excessive amounts of extractable anions, particularly chlorine, nitrate, phosphate and sulfate. The electrostatic dissipative polymers can be blended with a variety of base polymers to form plastic alloys, which in turn can be utilized to form articles useful in the manufacture of electrostatic sensitive electronic devices.
- Full text
- View on Google Patents
Claims (20)
- A polymer useful in forming a plastic alloy for use with an electronic device, said polymer comprising: an effective amount of a salt for electrostatic dissipation, wherein said salt is one or more of lithium trifluoromethane sulfonimide, LiSO 3 CF 3, LiC(SO 2 CF 3) 3, and LiMR 4 wherein M is Al or B, and R is a halogen, alkyl or aryl group; and an effective amount of a co-solvent for said salt; and wherein said polymer has a surface resistivity of from about 1.0×10 6 ohm/square to about 1.0×10 10 ohm/square as measured by ASTM D-257, and wherein said polymer has a volume resistivity of from about 1.0×10 6 ohm-centimeter to about 1.0×10 10 ohm-centimeter as measured by ASTM D-257; and wherein said polymer has less than about 8,000 parts per billion total extractable anions measured from the group of all four of chlorine anions, nitrate anions, phosphate anions and sulfate anions, and less than about 1,000 parts per billion of said chlorine anions, less than about 100 parts per billion of said nitrate anions, less than about 6,000 parts per billion of said phosphate anions, and less than about 1,000 parts per billion of said sulfate anions.
- The polymer of claim 1, in which said polymer has less than about 7,200 parts per billion total extractable anions measured from the group of all four of chlorine anions, nitrate anions, phosphate anions, and sulfate anions, and less than about 700 parts per billion of said chlorine anions, less than about 90 parts per billion of said nitrate anions, less than about 5,700 parts per billion of said phosphate anions, and less than about 750 parts per billion of said sulfate anions.
- The polymer of claim 2, in which said polymer has less than about 6,200 parts per billion total extractable anions measured from the group of all four of chlorine anions, nitrate anions, phosphate anions, and sulfate anions, and less than about 350 parts per billion of said chlorine anions, less than about 75 parts per billion of said nitrate anions, less than about 5,350 parts per billion of said phosphate anions, and less than about 450 parts per billion of said sulfate anions.
- The polymer of claim 1, in which said polymer has a volume resistivity of from about 1.0×10 6 to about 1.0×10 9.
- The polymer of claim 4, in which said polymer has a volume resistivity of from about 1.0×10 7 to about 1.0×10 8.
- The polymer of claim 1, in which said polymer has a surface resistivity of from about 1.0×10 6 to about 1.0×10 9.
- The polymer of claim 6, in which said polymer has a surface resistivity of from about 1.0×10 7 to about 1.0×10 8.
- The polymer of claim 1, in which said effective amount of said salt is at least about 0.1 parts based on 100 parts of said polymer.
- The polymer of claim 8, in which said effective amount of said salt is at least about 0.25 parts.
- The polymer of claim 9, in which said effective amount of said salt is at least about 0.75 parts.
- The polymer of claim 1, in which said effective amount of said co-solvent is at least about 0.1 parts based on 100 parts of said polymer.
- The polymer of claim 11, in which said effective amount of said co-solvent is at least about 0.5 parts based on 100 parts of said polymer.
- The polymer of claim 12, in which said effective amount of said co-solvent is at least about 1 part based on 100 parts of said polymer.
- The polymer of claim 1, in which said co-solvent is one or more of ethylene carbonate, propylene carbonate, dimethyl sulfoxide, tetramethylene sulfone, tri- and tetraethylene glycol dimethyl ether, gamma butyrolactone, or N-methyl-2-pyrrolidone.
- The polymer of claim 14, in which said co-solvent is ethylene carbonate.
- The polymer of claim 1, in which said salt is lithium trifluoromethane sulfonimide.
- The polymer of claim 1, in which said polymer is the reaction product of a chain extended polyether oligomer.
- The polymer of claim 17 in which said polymer is one or more of thermoplastic polyurethane, polyether amide block copolymer, or polyetherester block copolymers.
- The polymer of claim 18, in which said polymer comprises thermoplastic polyurethane.
- The polymer of claim 1, in which said polymer has a static decay time at 1000 V and 51 percent relative humidity of from about 1.0×10 -1 to about 2.5×10 -1 as measured using a charged plate monitor; and in which said polymer has a static decay time at 5000 V and 11.5 percent relative humidity of from about 1.0×10 -1 to about 2.5×10 -1 as measured by FTMS 1001C.
Description
1. Field of the Invention
The present invention relates to electrostatic dissipative polymers, and in particular to salt-modified electrostatic dissipative polymers reacted from polyether oligomers. More particularly, the present invention is directed to salt-modified electrostatic dissipative polymers reacted from polyether oligomers, which exhibit relatively low surface and volume resistivities, but which are generally free of excessive amounts of extractable anions.
2. Background Art
The formation and retention of charges of static electricity on the surface of most plastics is well known. Plastic materials have a significant tendency to accumulate static electrical charges due to low electrical conductivity. This type of formation and retention of charges of static electricity can be problematic. The presence of static electrical charges on sheets of thermoplastic film, for example, can cause the sheets to adhere to one another thus making their separation for further processing more difficult. Moreover, the presence of static electrical charges causes dust to adhere to items packaged in a plastic bag for example, which may negate any sales appeal.
The increasing complexity and sensitivity of microelectronic devices makes the control of static discharge of particular concern to the electronics industry. Even a low voltage discharge can cause severe damage to sensitive devices. The need to control static charge buildup and dissipation often requires the entire assembly environment for these devices to be constructed of partially conductive materials.