MLchartDataset catalogue

Patent · US8076230B2 · B2 · US

Method of forming self-aligned contacts and local interconnects

(11) Publication number
US8076230B2
(21) Application number
12/505,669
(22) Filing date
2009-07-20
(30) Priority date
2005-07-01
(43) Publication date
2011-12-13
(45) Date of grant
2011-12-13
(51) IPC
H10P 14/40
(52) CPC
  • H10W Generic packages, interconnections, connectors or other constructional details of devices covered by class H10: 20/069, 20/0698
  • H10D Inorganic electric semiconductor devices: 64/021
(73) Assignee
Macronix International Co Ltd
(72) Inventors
An Chyi Wei
(54) Title
Method of forming self-aligned contacts and local interconnects
(57) Abstract

A method for simultaneous formation of a self-aligned contact of a core region and a local interconnect of a peripheral region of an integrated circuit includes etching a cap dielectric layer to simultaneously form a hole in the core region and a trench in the peripheral region of the cap dielectric layer, etching a dielectric layer to simultaneously form a hole in the core region and a trench in the peripheral region of the dielectric layer of the dielectric layer, etching a liner layer simultaneously on a shoulder of sidewall spacers associated with the hole and with the trench of the dielectric layer without etching the liner layer at a bottom area of the hole and the trench, performing an oxygen flushing to remove polymer residues, and etching simultaneously through the liner layer that lines the bottom area of the hole and the trench.

Full text
View on Google Patents

Claims (30)

  1. A method for formation of a contact and a local interconnect of an integrated circuit, comprising the steps of: etching a cap dielectric layer to form a hole and a trench of the cap dielectric layer; etching a dielectric layer to form a hole and a trench of the dielectric layer of the dielectric layer; etching a liner layer on a shoulder of sidewall spacers associated with the hole and with the trench of the dielectric layer without etching the liner layer at a bottom area of the hole and the trench; performing an oxygen flushing to remove polymer residues; and etching through the liner layer that lines the bottom area of the hole and the trench.
  2. The method of claim 1, wherein the etching of the dielectric layer and the etching of the liner layer have a high selectivity with respect to the dielectric layer and the sidewall spacers.
  3. The method of claim 1, wherein the cap dielectric layer includes silicon oxynitride (SiON) and tetra-ethyl-ortho silicate (TEOS).
  4. The method of claim 1, wherein the dielectric layer includes boronphosphosilicate glass (BPSG).
  5. The method of claim 1, wherein the sidewall spacers include silicon nitride (SiN).
  6. The method of claim 1, wherein the etching of the dielectric layer includes an etchant comprising Ar, C 4 F 6, and O 2.
  7. The method of claim 6, wherein the etching of the dielectric layer includes an etchant comprising Ar at a flow rate between 200 to 300 sccm, and C 4 F 6 at a flow rate between 10 to 13 sccm.
  8. The method of claim 1, wherein the etching of the liner layer includes an etchant-comprising Ar, C 4 F 6, and O 2.
  9. The method of claim 8, wherein the etching of the liner layer includes an etchant comprising Ar at a flow rate between 200 to 300 sccm, and C 4 F 6 at a flow rate between 10 to 13 sccm.
  10. A method of fabricating a semiconductor device on a semiconductor substrate, comprising the steps of: forming a gate structure on the semiconductor substrate; forming sidewall spacers around the gate structures; forming a silicon nitride (SiN) liner layer over the semiconductor substrate; forming a dielectric layer over the semiconductor substrate; forming a photoresist pattern to define a hole associated with at least one self-aligned contact and a trench associated with a local interconnect opening; and etching the dielectric layer and the SiN liner layer before etching the portion of the SiN liner layer that lines a bottom area of the hole and the trench to form at least one self-aligned contact and local interconnect opening.
  11. The method of claim 10, wherein the etching has a high selectivity with respect to the dielectric layer and the sidewall spacers.
  12. The method of claim 10, wherein the semiconductor device includes a non-volatile memory.
  13. The method of claim 12, wherein the non-volatile memory includes a flash memory.
  14. The method of claim 12, wherein the gate-structure includes a multi-layered gate structure.
  15. The method of claim 10, wherein the dielectric layer includes silicon oxynitride (SiON), tetra-ethyl-ortho silicate (TEOS), and boronphosphosilicate glass (BPSG).
  16. The method of claim 10, wherein the sidewall spacer layer includes silicon nitride (SiN).
  17. The method of claim 10, wherein the etching includes an etchant comprising Ar, C 4 F 6, and O 2.
  18. The method of claim 17, wherein the etching includes an etchant comprising Ar at a flow rate between 200 to 300 sccm, and C 4 F 6 at a flow rate between 10 to 13 sccm both for about 45 seconds.
  19. The method of claim 18, wherein the etching further includes an etchant comprising Ar at a flow rate between 200 to 300 sccm, and C 4 F 6 at a flow rate between 10 to 13 sccm both for about 60 seconds.
  20. A method of fabricating a semiconductor device on a semiconductor substrate, comprising the steps of: forming sidewall spacers around a gate-structure on the semiconductor substrate in a core region and around a gate-structure in a peripheral region on the semiconductor substrate, thereby forming a hole and a trench respectively; forming a silicon nitride (SiN) liner layer and a dielectric layer on the substrate; and etching the dielectric layer and the SiN liner layer on the sidewall spacers before etching a portion of the SiN liner layer that lines a bottom area of the hole and the trench to form a self-aligned contact and a local interconnect opening.
  21. The method of claim 20, wherein the etching has a high selectivity with respect to the dielectric layer and the sidewall spacers.
  22. The method of claim 20, wherein the semiconductor device includes a non-volatile memory.
  23. The method of claim 22, wherein the non-volatile memory includes a flash memory.
  24. The method of claim 22, wherein the gate-structure includes a multi-layered gate structure.
  25. The method of claim 20, wherein the dielectric layer includes silicon oxynitride (SiON), tetra-ethyl-ortho silicate (TEOS), and boronphosphosilicate glass (BPSG).
  26. The method of claim 20, wherein the sidewall spacer layer includes silicon nitride (SiN).
  27. The method of claim 20, wherein the etching includes an etchant comprising Ar, C 4 F 6, and O 2.
  28. The method of claim 20, wherein the etching includes an etchant comprising Ar at a flow rate between 200 to 300 sccm, and C 4 F 6 at a flow rate between 10 to 13 sccm both for about 45 seconds.
  29. The method of claim 28, wherein the etching further includes an etchant comprising Ar at a flow rate between 200 to 300 sccm, and C 4 F 6 at a flow rate between 10 to 13 sccm both for about 60 seconds.
  30. A method of fabricating a semiconductor device on a semiconductor substrate, comprising the steps of: forming sidewall spacers around a gate-structure on the semiconductor substrate in a core region and around a gate-structure in a peripheral region on the semiconductor substrate, thereby forming a hole in a source region of the substrate and a trench in a drain region of the substrate, respectively; forming a silicon nitride (SiN) liner layer and a dielectric layer on the substrate; and etching the dielectric layer and the SiN liner layer on the sidewall spacers before etching a portion of the SiN liner layer that lines a bottom area of the hole and the trench to form a self-aligned contact in the source region and a local interconnect opening in the drain region.

Description

1. Field of the Invention

The present invention relates to a method of fabricating semiconductor devices, and more particularly to forming self-aligned contacts and local interconnects of semiconductor devices.

2. Description of the Related Art

In recent years, the size of integrated circuit devices continues to decrease resulting in considerable increase of the packing densities for these devices. The performance of the integrated circuit devices also improves as a result while the manufacture costs have gone down as well.

However, the performance of denser integrated circuit devices could drop when smaller process parameters are used. Accordingly, the issue of maintaining or controlling the precision of contact windows is particularly important as the density of integrated circuit devices continues to increase for future generations of these devices. This etching control issue is even more critical for integrated circuit devices with multiple polysilicon layers. Therefore, a so-called self-aligned contact (SAC) process which can reduce contact area is developed to deal with this issue.

Various SAC processes exist today. For example, U.S. Pat. No. 6,271,081 to Kinoshita et al. (the entire disclosure of which is herein incorporated by reference) provides a method of forming self-aligned contacts and local interconnects using self-aligned local interconnects. Referring now more particularly to FIGS. 1A-1D, there are illustrated the cross sectional views of the SAC process disclosed by Kinoshita et al.