MLchartDataset catalogue

Patent · US10923617B2 · B2 · US

Methods for fabricating thin film III-V compound solar cell

(11) Publication number
US10923617B2
(21) Application number
13/165,318
(22) Filing date
2011-06-21
(30) Priority date
2007-07-03
(43) Publication date
2021-02-16
(45) Date of grant
2021-02-16
(51) IPC
H01L 31/0232; H01L 31/0304; H01L 31/078; H01L 31/0687; H01L 31/18
(52) CPC
  • H10F Inorganic semiconductor devices sensitive to infrared radiation, light, electromagnetic radiation of shorter wavelength or corpuscular radiation: 71/1276, 10/1425, 71/1272, 71/1395
  • H01L Semiconductor devices; electric solid state devices not otherwise provided for: 31/06875, 31/1844, 31/1852, 31/1896
  • Y02E Reduction of greenhouse gas [ghg] emissions, related to energy generation, transmission or distribution: 10/544
(73) Assignee
Microlink Devices Inc
(72) Inventors
Noren Pan; Glen Hillier; Duy Phach Vu; Rao Tatavarti; Christopher Youtsey; David McCallum; Genevieve Martin
(54) Title
Methods for fabricating thin film III-V compound solar cell
(57) Abstract

The present invention utilizes epitaxial lift-off in which a sacrificial layer is included in the epitaxial growth between the substrate and a thin film III-V compound solar cell. To provide support for the thin film III-V compound solar cell in absence of the substrate, a backing layer is applied to a surface of the thin film III-V compound solar cell before it is separated from the substrate. To separate the thin film III-V compound solar cell from the substrate, the sacrificial layer is removed as part of the epitaxial lift-off. Once the substrate is separated from the thin film III-V compound solar cell, the substrate may then be reused in the formation of another thin film III-V compound solar cell.

Full text
View on Google Patents

Claims (25)

  1. A method for fabricating one or more thin film multi-junction III-V compound solar cells on a substrate having a diameter corresponding to a 6 inch wafer, the method comprising the steps of: providing a substrate having a diameter corresponding to a 6 inch wafer; forming a sacrificial layer on the substrate; forming a plurality of active layers of one or more multi-junction III-V compound solar cells on the sacrificial layer, each of the plurality of active layers having an associated band gap energy, at least one of the plurality of active layers being lattice mismatched with the substrate, each of the one or more multi-junction III-V compound solar cells having at least three junctions; forming a support backing layer directly on a last formed active layer of the plurality of active layers, the support backing layer consisting of one or more metal or metals, the metal or metals comprising nickel; removing the sacrificial layer from between the plurality of active layers and the substrate by epitaxial lift off to separate the plurality of active layers and the support backing layer from the substrate on a 6 inch wafer-sized scale, wherein the support backing layer is the outermost layer during removal of the sacrificial layer from between the plurality of active layers and the substrate; and wherein the support backing layer provides structural support for the plurality of active layers during separation of the plurality of active layers and the support backing layer from the substrate; and processing the plurality of active layers and the support backing layer separated from the substrate on a 6 inch wafer-sized scale to form the one or more thin film multi-junction III-V compound solar cells.
  2. The method of claim 1, wherein the formed one or more thin film multi-junction III-V compound solar cells are flexible.
  3. The method of claim 1, wherein the substrate is formed of a III-V compound.
  4. The method of claim 1, wherein the substrate had been previously used in a fabrication process of another thin film III-V compound solar cell.
  5. The method of claim 3, wherein the substrate is formed of at least one of Gallium Arsenide (GaAs) and Indium Phosphide (InP).
  6. The method of claim 1, wherein the sacrificial layer is formed from at least one of Aluminum Gallium Arsenide (Al x Ga 1·x As), Indium Aluminum Arsenide (In x Al 1·x As), Aluminum Phosphide Antimonide (AlP x Sb 1·x) and Aluminum Arsenide Antimonide (A 1 As,Sb 1·x).
  7. The method of claim 1, wherein each of the plurality of active layers is formed from a III-V compound.
  8. The method of claim 7, wherein the III-V compound from which any of the plurality of active layers is formed is selected from the group consisting of Gallium Arsenide (GaAs), Gallium Iridium Phosphide (Ga 1·x In x P), Gallium Indium Arsenide (Ga 1·x In x As), Indium Phosphide (InP), Gallium Iridium Arsenide Phosphide (Ga 1·x In x As 1−y P y), and Aluminum Gallium Iridium Phosphide ((Al x Ga 1−x) 1−y In y P).
  9. The method of claim 1, wherein removing the sacrificial layer from between the plurality of active layers and the substrate by epitaxial lift off comprises: immersing the substrate, the sacrificial layer, the plurality of active layers, and the support backing layer in an acid etching environment to dissolve the sacrificial layer.
  10. The method of claim 1, further comprising the steps of, applying surface metallization to a surface of an active layer in the plurality of active layers that is exposed and facing away from the support backing layer after removal of the sacrificial layer; and applying an antireflection coating to the surface of the active layer that is exposed and facing away from the support backing layer.
  11. The method of claim 1, wherein providing the substrate having the diameter corresponding to a 6 inch wafer comprises receiving a substrate previously used to form a III-V compound solar cell.
  12. The method of claim 1, wherein the support backing layer has a thickness of 10-50 μm.
  13. The method of claim 1, wherein the processing of the plurality of active layers and the support backing layer separated from the substrate having the diameter corresponding to the 6 inch wafer includes forming a plurality of thin film multi-junction III-V compound solar cells.
  14. The method of claim 1, wherein the support backing layer is the final layer formed on the substrate prior to removal of the sacrificial layer.
  15. The method of claim 1, wherein the support backing layer has a first surface that remains in contact with the last formed active layer of the plurality of active layers and a second surface facing away from the plurality of active layers that remains exposed to an external environment during removal of the sacrificial layer and separation of the plurality of active layers and the support backing layer from the substrate.
  16. The method of claim 1, wherein the support backing layer provides structural support for the one or more thin film multi-junction III-V compound solar cells after separation from the substrate.
  17. The method of claim 1, wherein a surface of the support backing layer facing away from the substrate is exposed to an etching environment during removal of the sacrificial layer from between the plurality of active layers and the substrate.
  18. The method of claim 1, wherein the support backing layer is formed directly on the last formed active layer of the plurality of active layers by plating, evaporation or sputtering.
  19. The method of claim 1, wherein the plurality of active layers includes at least: a first active layer comprising GaAs; and a second active layer comprising InGaP.
  20. The method of claim 1, wherein the plurality of active layers includes: a first active layer comprising InGaAs; a second active layer comprising GaAs or a compound comprising Ga and As; and a third active layer comprising InGaP or AlGaInP.
  21. The method of claim 1, wherein the support backing layer comprises a plurality of metal sublayers; wherein forming the support backing layer directly on the last formed active layer of the plurality of active layers comprises forming a first metal sublayer directly on the last formed active layer of the plurality of active layers and forming other metal sublayers of the plurality of metal sublayers over the last formed active layer of the plurality of active layers; and wherein at least one of the plurality of metal sublayers comprises nickel.
  22. The method of claim 21, wherein at least one of the plurality of metal sublayers comprises copper.
  23. The method of claim 1, wherein each of the one or more thin film III-V compound solar cells has four junctions.
  24. The method of claim 1, wherein each of the one or more thin film III-V compound solar cells has five junctions.
  25. The method of claim 1, wherein each of the one or more thin film III-V compound solar cells has at least five junctions.

Description

The present invention concerns photovoltaic devices. More specifically, the present invention concerns compound based photovoltaic devices and epitaxial lift-off methodologies in the fabrication of III-V compound based photovoltaic devices.

Currently, III-V compound based photovoltaic devices are epitaxially grown on substrates and remain affixed thereto throughout fabrication and deployment as a solar cell. In many cases, the substrates can be approximately 150 μm thick. Having substrates with such thickness may introduce a number of undesirable consequences for a solar cell.

One such undesirable consequence is weight. The thick substrate can make up a large percentage of the overall weight of the resulting solar cell. In certain applications, such as space applications, weight and size of a solar cell can be significant given the liftoff capability of the selected launch vehicle.

Another undesirable consequence is poor thermal conductivity. The substrate increases the thermal impedance between the solar cell and a heat sink on which the substrate and solar cell may be mounted. The increased thermal impedance results in higher junction temperatures in the solar cell, which, in turn, reduces the efficiency of the solar cell.

Another undesirable consequence is environmental impact. The substrate serves no purpose other than as a mechanical support for the solar cell. In addition, to achieve a substrate thickness of approximately 150 μm, it is typically necessary to remove, mechanically or chemically, part of the substrate, which amounts to further waste.