Patent · US6636313B2 · B2 · US
Method of measuring photoresist and bump misalignment
- (11) Publication number
- US6636313B2
- (21) Application number
- 10/045,413
- (22) Filing date
- 2002-01-12
- (30) Priority date
- 2002-01-12
- (43) Publication date
- 2003-10-21
- (45) Date of grant
- 2003-10-21
- (51) IPC
- G01B 11/27; G03F 7/20
- (52) CPC
- G03F Photomechanical production of textured or patterned surfaces, e.g. for printing, for processing of semiconductor devices; materials therefor; originals therefor; apparatus specially adapted therefor: 7/70633
- G01B Measuring length, thickness or similar linear dimensions; measuring angles; measuring areas; measuring irregularities of surfaces or contours: 11/272
- H10W Generic packages, interconnections, connectors or other constructional details of devices covered by class H10: 72/012, 72/923, 72/9232, 72/9415, 72/985
- (73) Assignee
- Taiwan Semiconductor Manufacturing Co TSMC Ltd
- (72) Inventors
- Yen-Ming Chen; Chia-Fu Lin; Kai-Ming Ching; Chao-Yuan Su; Hsin-Hui Lee; Li-Chih Chen
- (54) Title
- Method of measuring photoresist and bump misalignment
- (57) Abstract
A method including the acts of providing a semiconductor device having a plurality of misalignment ruler markers formed therein for measuring removable layer opening misalignment in the X and Y directions, a bond pad and the passivation layer with an opening therein down to the bond pad. A removable layer is formed over the semiconductor device and includes an opening therein down to the bond pad. Preferably this action includes depositing, patterning and developing a dry photoresist film layer over the semiconductor device with an opening therein down to the bond pad. The next act includes measuring the misalignment of the opening in the passivation layer by counting the number of misalignment ruler markers visibly exposed by the opening in the X-direction and also the Y-direction.
- Full text
- View on Google Patents
Claims (20)
- A method comprising: (a) providing a semiconductor device having a plurality of spaced apart misalignment ruler markers formed therein for measuring the misalignment of an opening in a removable layer in the X and Y directions, and a bond pad formed therein; (b) depositing a removable layer over the semiconductor device, and wherein the removable layer includes an opening formed therein down to the bond pad; and (c) measuring the misalignment of the opening in the removable layer by counting the number of misalignment ruler markers exposed by the opening in the removable layer in the X-direction and in the Y- direction.
- A method as set forth in claim 1 wherein the plurality of misalignment ruler markers includes at least a first set of spaced apart lines.
- A method as set forth in claim 1 wherein each of the misalignment ruler markers comprises the same material as the bond pad.
- A method as set forth in claim 1 wherein the plurality of this alignment ruler markers comprises first, second, third, and fourth sets of spaced apart lines, and wherein the first set of spaced apart lines is positioned on an opposite side of the bond pad from the third set of spaced apart lines so that the first and the third sets of spaced apart lines are usable to measure the misalignment of the opening in the removable layer in the Y- direction, and wherein the second set of spaced apart lines is positioned on an opposite side of the bond pad from the fourth set of spaced apart lines so that the second and fourth set of spaced apart lines are usable to measure the misalignment of the opening in the removable layer in the X- direction.
- A method as set forth in claim 4 wherein the spaced apart lines of each set are spaced apart from each other an equal distance.
- A method as set forth in claim 4 wherein the spaced apart lines of each set are spaced apart from each other 1 micron.
- A method as set forth in claim 1 wherein the removal layer comprises a photoresist.
- A method as set forth in claim 1 wherein the removable layer comprises a dry film photoresist.
- A method as set forth in claim 1 further comprising the act of determining whether the measured misalignment of the opening in the removable layer in each of the X- direction and the Y- direction are within an acceptable tolerance range.
- A method as set forth in claim 1 further comprising the acts of: (d) determining whether the measured misalignment of the opening in the removable layer in each of the X-direction and the Y-direction are within an acceptable tolerance range; (e) and if the measured misalignment is outside of the acceptable tolerance range then: (f) removing the removable layer; (g) adjusting the process equipment and tools to compensate for the measured misalignment of the opening in the removable layer; and (h) repeating the acts b-d until the measured misalignment is within the acceptable tolerance range.
- A method as set forth in claim 1 further comprising the acts of: (d) determining whether the measured misalignment of the opening in each of the X-direction and the Y-direction are within an acceptable tolerance range; (i) if the misalignment is within the acceptable tolerance range then further comprising the acts of: (j) depositing an under bump metallurgy into the opening in the removable layer; (k) depositing an electrically conductive bump material into the opening in the removable layer and over the under bump metallurgy; (1) removing the removable layer; and (m) reflowing the electrically conductive bump material to form a bump on the semiconductor device.
- A method as set forth in claim 1 further comprising the act of viewing the semiconductor device through an optical microscope in order to perform the act of counting the number of misalignment ruler markers.
- A method comprising: (a) providing a semiconductor device having a plurality of spaced apart misalignment ruler markers formed therein for measuring the misalignment of an opening in a removable layer in the X and Y directions, and a bond pad formed therein; (b) depositing a removable layer over the semiconductor device, and wherein the removable layer includes an opening formed therein down to the bond pad; (c) measuring the misalignment of the opening in the removable layer by counting the number of misalignment ruler markers exposed by the opening in the removable layer in the X- direction and in the Y- direction; (d) determining if the measured misalignment is within an acceptable tolerance range; (e) if the measured misalignment is outside of the acceptable tolerance range, and then removing the removable layer, adjusting the process equipment and tools to compensate for the measured misalignment of the opening in the removable layer, and repeating acts b-d until the measured misalignment of the opening is within acceptable tolerance range; (f) if the measured misalignment of the opening is within an acceptable tolerance range then performing the acts g-i; (g) depositing an electrically conductive bump material into the opening in the removable layer; (h) removing the removable layer; and (i) reflowing the electrically conductive bump material to form a bump on the semiconductor device.
- A method as set forth in claim 13 wherein the removable layer comprises a photoresist layer.
- A method as set forth in claim 13 wherein the removable layer comprises a dry film photoresist layer.
- A method as set forth in claim 13 wherein the plurality of misalignment ruler markers includes at least a first set of spaced apart lines.
- A method as set forth in claim 13 wherein each of the misalignment ruler markers comprises the same material as the bond pad.
- A method as set forth in claim 13 wherein the plurality of this alignment ruler markers comprises first, second, third, and fourth sets of spaced apart lines, and wherein the first set of spaced apart lines is positioned on an opposite side of the bond pad from the third set of spaced apart lines so that the first and the third sets of spaced apart lines are usable to measure the misalignment of the opening in the removable layer in the Y-direction, and wherein the second set of spaced apart lines is positioned on an opposite side of the bond pad from the fourth set of spaced apart lines so that the second and fourth sets of spaced apart lines are usable to measure the misalignment of the opening in the removable layer in the X-direction.
- A method as set forth in claim 18 wherein the spaced apart lines of each set are spaced apart from each other an equal distance.
- A method as set forth in claim 18 wherein the spaced apart lines of each set are spaced apart from each other 1 micron.
Description
This invention relates to a method of making a bump on a substrate, and more particularly, to a method of making a bump on a substrate using a unique method of measuring photoresist and bump misalignment.
A flip chip microelectronic assembly includes a direct electrical connection of face down (that is, “flipped”) electronic components onto substrates, such as ceramic substrates, circuit boards, or carriers using conductive bump bond pads of the chip. Flip chip technology is quickly replacing older wire bonding technology that uses face up chips with a wire connected to each pad on the chip.
The flip chip components used in flip chip microelectronic assemblies are predominantly semiconductor devices, however, components such as passive filters, detector arrays, and MEM devices are also being used in flip chip form. Flip chips are also known as “direct chip attach” because the chip is directly attached to the substrate, board, or carrier by the conductive bumps.
The use a flip chip packaging has dramatically grown as a result of the flip chip's advantages in size, performance, flexibility, reliability, and cost over other packaging methods and from the widening availability of flip chip materials, equipment and services. In some cases, the elimination of old technology packages and bond wires may reduce the substrate or board area needed to secure the device by up to 25 percent, and may require far less height. Further, the weight of the flip chip can be less than 5 percent of the old technology package devices.